Kokohu Mapu-Welded Koeko Mahanga-Screw Barrel
  • Kokohu Mapu-Welded Koeko Mahanga-Screw BarrelKokohu Mapu-Welded Koeko Mahanga-Screw Barrel

Kokohu Mapu-Welded Koeko Mahanga-Screw Barrel

Ko nga awaawa helical o te Alloy Spray-Welded Conical Twin-Screw Barrel me te papa o roto o te pakitara o te oko kua whakakikoruatia ki te paparanga o te koranu tungsten carbide-atete teitei me te waikura i roto i te hangarau rehu rehu. He nui ake i te 5-8 nga wa o te whakamarumaru o te kakahu o nga papa nitriding noa.
Whakatauranga: 5.0
(Tatau Whakatauranga: 1)

Ahuatanga Hua me te Tono

1.Alloy rehu-wea paiherea koeko mahanga oko mahanga , me te ratonga ora roa rawa atu, I te wa e mahi ana me te aukati kakahu teitei, he roa ake tona oranga i nga waahanga nitrided. Ma tenei ka tino whakaiti i te waa mo te whakakapi me te whakarei ake i te whakamahinga taputapu me te pai o te whakaputa.

2.Double tīwiri, ki te mahi pūmau me te putanga tiketike.Ensured wā roa-rite rite i roto i te pānga plasticization, rōrahi extrusion me te kounga hua.

3.Tungsten koranu rehu rehu fehokotaki'anga ka taea e tōtika te hapai i te hau ha'iriiri hanga i roto i te tukatuka o ngā rauemi pērā i PVC me te hunga kei roto halogen retardants mura, me te ātete i te kino ngā i meinga e "waikura + kakahu".

4.Bimetallic conical twin-screw Ka whakamahia ki te PVC pakeke me te ngohengohe, ki te whakakii i nga kirihou miihini, ki nga paipa wai ahumahi, ki te WPC, ki nga papa rakau-kirihou PVC, ki nga papa pahuka, ki nga taera kapia, ki te masterbatches me te hanga masterbatches tae.

Alloy Spray-Welded Conical Twin-Screw BarrelAlloy Spray-Welded Conical Twin-Screw BarrelAlloy Spray-Welded Conical Twin-Screw Barrel

Nga Taipitopito Whakaputa

1. He pai te mahi: te kai pai, te kutikuti ngawari, me te hanga pehanga

2. Kohanga rehu fehokotaki'anga koeko mahanga oko tīwiri. Ko nga tere hurihuri o nga tira e rua i roto i te waahi kaa he rereke, e taea ai e ratou te whiti tetahi ki tetahi, me te aukati i nga rawa kei te piri me te pirau.

3. Te kaha o te whangai kai: Ko te waahanga whangai he nui te diameter me te riu riu hohonu, he mea tino pai mo te kawe i nga mea paura (penei i te paura PVC), he painga nui mo te hoahoa mahanga-rua.

4. Ko te pakitara o roto o te oko kei te whakauruhia ki te rino hauota, te raima koranu tungsten ranei, he nui rawa te mau o te kakahu me te aukati waikura, me te whakarite i te mahi tahi me te wiri.

Alloy Spray-Welded Conical Twin-Screw BarrelAlloy Spray-Welded Conical Twin-Screw Barrel
Tuku Uiui
Momo Whakapā
  • Wāhitau

    Poraka C,No.2 Wāhanga ki te Hauāuru,Xingzhou Avenue,Dinghai District,Zhoushan City,Zhejiang Province

Nau mai ki to maatau paetukutuku! Mo nga patai mo a maatau hua, raarangi utu ranei, waiho mai to imeera ki a maatau ka pa atu matou i roto i nga haora 24.
Whakatauranga:
5.0
X
Ka whakamahi matou i nga pihikete hei tuku atu ki a koe he wheako tirotiro pai ake, te tātari i te hokohoko o te pae me te whakawhaiaro i nga ihirangi. Ma te whakamahi i tenei pae, ka whakaae koe ki ta matou whakamahi pihikete. Kaupapahere Tūmataiti
WhakakahoreWhakaae