Konumohe-kirihou Pereti Whakarara Wiu Mahanga
  • Konumohe-kirihou Pereti Whakarara Wiu MahangaKonumohe-kirihou Pereti Whakarara Wiu Mahanga

Konumohe-kirihou Pereti Whakarara Wiu Mahanga

Ko te Nanhaiya Aluminum-Plastic Plate Parallel Twin Screws kei te hangaia mai i te kounga teitei o te 38CrMoAlA nitrided maitai, e tuku ana i te pai o te kakahu, te aukati waikura, me te kaha nui. Ka taea te whakarite i o maatau mahanga-rua ki o hiahia rauemi, tae atu ki te rino mahi wera, te rino mahi makariri, te maitai tere-tere, te rino paura HIP, me nga koranu PTA. I hoahoatia mo te mauroa me te tino pai, ka whakarite kia pumau te hanga me te kounga o nga hua. He nui te whakamahi i roto i te kirihou me te rapa extrusion, PVC, PE, PP, me etahi atu tukatuka polymer, me te whakahiato, te granulation, me te hanga rauemi teitei.
Whakatauranga: 5.0
(Tatau Whakatauranga: 1)

Nanhaiya Aluminum-Plastic Plate Parallel Twin Screws - High-Efficiency Extrusion mo Aluminium-Plastic Panels.He mea hangaia mo te tangohanga pai o te PVC me te PE composites. Ka taea te whakarite, te kakahu-atete, me te mahi nui, ka whakarite kia rewa rite, te putanga pumau, me te kounga o te hua.

Tawhā Hua (Whakaahuatanga)

Rauemi

38CrMoAlA

Te Maamaa o te Whakawera

HB260-320

Te Maamaa Nitriding

HV950-1000

Hohonu Nitriding

0.50-0.70mm

Te hauhautanga Nitriding

≤koeke 1

Te taratara

Ra0.4

Tiu Tiu

0.015mm

Maamaa Whakakikorua Chrome

HV≥950HV

Matotoru Chrome

0.05-0.10mm

Maamaa Bimetal

HRC60-65

Te Hohonu Bimetal

2.0-3.0mm

Ahuatanga Hua me te Tono

He pai te Whakapaipai me te Whakaranu Hangarite

1、Whakatutuki te kounga rewa rite, me te putanga teitei mo te konumohe-kirihou awhi, whakarite pūmau me te hanga pono.

2. Rauemi Roa Ka taea te whakarite

Ka taea te whakarite kia rite ki o hiahia rawa: te rino mahi wera, te rino mahi makariri, te maitai tere tere, te rino paura HIP, me nga koranu PTA - he pai mo te PVC, PE, me etahi atu rauemi hiato.

3. Te Kounga Pumau me te Iti Nga Koha

Ko te hoahoa takai tika e whakaiti ana i nga mirumiru, te rerekee o te rahi, me te wehenga paparanga, e whakaputa ana i te kounga teitei o te panui.

4. Te Ora Taputapu Whakaroa & Te Wa Whakaheke

Ka awhina nga kaakahu-kaahu-atete ki te whakaiti i te tiaki me te waatea, te whakapai ake i te pai o te whakaputa me te whakaheke i nga utu.

5. Hototahi ki te Paerewa & Whakaritenga Motuhake

He pai mo nga raina whakaputa paerewa me nga tohutoro rauemi motuhake, e whakarato ana i te putanga pono me nga panui konumohe-kirihou teitei.

Aluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin Screw

Nga Taipitopito Whakaputa

Ia Nanhaiya parallel twin screw barel is made with state-of-the-art CNC machining and high-precision grinding. Ko te mata orohia-whakaata ka whakaiti i te waku me te whakarei ake i te rere o nga rawa, ko nga rerenga tira whakapakeke, e parea ana e te nitriding, bimetallic koranu mata, kia mau tonu te mahi.

Aluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin ScrewAluminum-Plastic Plate Parallel Twin Screw
Tuku Uiui
Momo Whakapā
  • Wāhitau

    Poraka C,No.2 Wāhanga ki te Hauāuru,Xingzhou Avenue,Dinghai District,Zhoushan City,Zhejiang Province

Nau mai ki to maatau paetukutuku! Mo nga patai mo a maatau hua, raarangi utu ranei, waiho mai to imeera ki a maatau ka pa atu matou i roto i nga haora 24.
Whakatauranga:
5.0
X
Ka whakamahi matou i nga pihikete hei tuku atu ki a koe he wheako tirotiro pai ake, te tātari i te hokohoko o te pae me te whakawhaiaro i nga ihirangi. Ma te whakamahi i tenei pae, ka whakaae koe ki ta matou whakamahi pihikete. Kaupapahere Tūmataiti
WhakakahoreWhakaae